Analysis of the development of damage in a welded junction in the hot intermediate superheat steam duct of 800-MW generator units
Authors:E A Grin’  A E Anokhov
Institution:(1) JSC “All-Russian Thermotechnical Institute” (VTI), Moscow, Russia
Abstract:Data from a metallographic study of a damaged weld junction in a hot intermediate superheat steam duct and a computational model for crack development (in the damaged zone) by a creep mechanism are described. Anumerical calculation confirms the possibility of crack development to the known final size over a time of approximately 15,000 h, which corresponds to the operating time for the steam duct from the last time it was inspected until the time of a through fault, under conditions such that a 2.5-mm-deep surface crack (with a length of ∼50 mm along the surface) had been overlooked during this last inspection. Translated from élektricheskie Stantsii, No. 10, October 2008, pp. 29–35.
Keywords:welded junction  steam duct  damage  stress  crack  creep  stability
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号